Jnchdghwa Gold 2Set 7/11/14Mm Plumbing Repair Tools Plastic Ppr Repair Die Heads Welder Tool Welding Plastic Pipes Ppr Pipe Repair
Jnchdghwa
2: The first punch (long) and die (short) patch is installed on the fuser heat plate; 1: Choose good support specifications repair damaged mold parts according to size; 3: the fuser heated to a certain temperature (260-300 degrees); 4: Water pipes damaged by the site cleans the image shown above; the (long) punch inserted into the damaged site, and insert the special die (short) stick glue tube into the melt; 5: Well specific melt glue stick is inserted just melt quickly after Cooling Holes and other damage with a knife to cut the stick Glue And you are done., Manufacturer: Jnchdghwa